THE FURNITURE STRIPPING PROCESS - PAINTED BUFFET
BEFORE
TOP LAYER OF GREEN COMING UP
GETTING DOWN TO SECOND LAYER OF PAINT
SECOND LAYER COMING UP
DOWN TO WOOD
RINSED OFF AND DRYING